Nanoindentation is a technique used to measure the mechanical properties of materials at the nanoscale by pressing a sharp indenter into the surface of a specimen. This method provides valuable information on hardness, elastic modulus, and other mechanical characteristics, making it particularly useful in evaluating materials like polymers, metals, and ceramics. Its precision enables researchers to study materials that exhibit size-dependent properties, which is crucial for understanding behavior in nanotechnology applications.